ASTM A194 2HM heavy hex nuts for sour service
Hardness-limited carbon steel heavy hex nuts for B7M stud bolts in wet sour (H2S) service, every nut hardness tested to 237 HB maximum.
ASTM A194 Grade 2HM is a quenched and tempered medium carbon steel heavy hex nut, tempered at 1150 °F or above so its hardness stays between 159 and 237 HB (22 HRC maximum). It is the matching nut for B7M stud bolts in sour service, and Saudi Aramco SAES-L-109 pairs B7M with 2HM for wet sour service. JTE Fasteners supplies 2HM nuts with hardness results on the EN 10204 3.1 certificate.
- Material
- Medium carbon steel, quenched and tempered
- Min tempering
- 1150 °F (621 °C)
- Hardness
- 159–237 HB (22 HRC max)
- Proof stress
- 150 ksi (heavy hex)
- Hardness testing
- Every nut
- Marking
- 2HM and maker’s mark
- Pairs with
- ASTM A193 B7M
- Sour service
- NACE MR0175 / ISO 15156



A194 nut grades compared
The five heat-treated grades used on Saudi flanges, side by side.
| Grade | Material | Min tempering | Hardness | Proof stress (heavy hex) | Typical stud |
|---|---|---|---|---|---|
| 2H | Medium carbon steel, quenched and tempered | 850 °F (454 °C) | 24–38 HRC | 175 ksi (1,207 MPa) | A193 B7 |
| 2HM | Medium carbon steel, quenched and tempered, hardness-limited | 1150 °F (621 °C) | 159–237 HB (22 HRC max) | 150 ksi (1,034 MPa) | A193 B7M |
| 4 | Carbon-molybdenum steel, quenched and tempered (removed from A194 in 2017) | 1100 °F (593 °C) | 24–38 HRC | 175 ksi (1,207 MPa) | A193 B16, A320 L7 |
| 7 | Chromium-molybdenum alloy steel, quenched and tempered | 1100 °F (593 °C) | 24–38 HRC | 175 ksi (1,207 MPa) | A320 L7, A193 B16, A193 B7 |
| 7M | Chromium-molybdenum alloy steel, quenched and tempered, hardness-limited | 1150 °F (621 °C) | 159–237 HB (22 HRC max) | 150 ksi (1,034 MPa) | A320 L7M |
Values from ASTM A194 for heavy hex nuts (coarse and 8-pitch threads); 24–38 HRC is about 248–352 HB. Always order to the edition your specification names.
Saudi Arabia requirements for 2HM nuts
2HM is the sour-service nut in Saudi Aramco SAES-L-109, but only where the bolting can actually meet the sour fluid.
| Requirement | What it means |
|---|---|
| Wet sour service (SAES-L-109, Table 5) | B7M studs with 2HM nuts. |
| Where it applies (13.2.3) | Only where bolting is directly or potentially exposed to the sour fluid, such as buried, insulated or shielded flanges. |
| Sour service definition | As defined in Saudi Aramco SAES-L-133. |
| Hardness limit | 22 HRC / 237 HB maximum, in line with NACE MR0175 / ISO 15156. |
| Coated sour bolting (13.3) | A coating to 09-SAMSS-107 does not change the grade: the nut stays 2HM. |
| Vendor status | JTE Fasteners is ISO 9001 certified and a registered Saudi Aramco and SABIC vendor. |
Summarised from Saudi Aramco SAES-L-109 (29 January 2018 edition). Always work to the current revision, the plant specification and your purchase order.
Where 2HM nuts are used
Wherever wet H2S can reach the bolting.
Sour gas piping
Flanges in H2S-bearing gas and condensate lines.
Sour water units
Strippers and sour water piping in refineries.
Insulated and buried flanges
Joints where a leak can wet the bolting.
B7M / 2HM sets
Studs and nuts supplied and certified together.
Coated sour sets
PTFE-coated B7M studs with 2HM nuts.
Hardness records
Hardness results reported on the certificate.
Tested before it ships
Every 2HM nut is hardness tested; nuts above the limit are rejected.
- 159–237 HB
- 22 HRC maximum
- Marked 2HM
- Matched to B7M studs
Documents with every order
Each lot is traceable to its heat and hardness tested.
- EN 10204 3.1 with heat number
- Hardness results on the certificate
- 3.2 with third-party inspection
- PMI on request
A194 2HM nut questions
What is an ASTM A194 2HM nut?
A hardness-limited heavy hex nut of quenched and tempered medium carbon steel, 159–237 HB (22 HRC maximum), with a 150 ksi proof stress, used with B7M studs in sour service.
Why does sour service need 2HM instead of 2H?
Hard steel can crack under stress in wet H2S (sulfide stress cracking). Limiting hardness to 22 HRC, as NACE MR0175 / ISO 15156 requires, makes 2HM resistant; a 2H nut can be up to 38 HRC.
Which stud goes with a 2HM nut?
ASTM A193 B7M, which is also hardness-limited.
Is a 2HM nut weaker than a 2H nut?
Yes: its proof stress is 150 ksi against 175 ksi. B7M studs also have a lower minimum yield (80 ksi) than B7 (105 ksi), so the joint is designed and tightened for that.
Does Saudi Aramco require 2HM on every sour line?
No. SAES-L-109 section 13.2.3 requires wet sour bolting only where the bolts are directly or potentially exposed to the fluid.
How is a 2HM nut marked?
With “2HM” and the manufacturer’s identification mark.
Related
B7M stud bolts
The sour-service stud for 2HM nuts.
2H vs 2HM
How the two nuts differ.
Nut compatibility chart
Which nut goes with which bolt.
Sour service bolting?
Send size and quantity for B7M / 2HM sets: hardness tested, marked and certified.