Anti-seize compound, thread sealants and PTFE tape
Copper, nickel, metal-free and moly anti-seize pastes for flange studs, anaerobic sealants and threadlockers, PTFE thread seal tape and pipe dope. Sourced from established manufacturers and supplied from Al Jubail with your bolting.
An anti-seize compound is a grease filled with metal, graphite or ceramic solids. It stops threads galling during tightening and seizing in service. Copper grades suit carbon steel, nickel and metal-free grades suit stainless steel and high temperature, and moly pastes give the lowest friction. Every lubricant changes the nut factor K, so bolt torque must be calculated for the product used. Thread sealants are a different job: anaerobic resins, PTFE tape and pipe dope seal tapered pipe threads.
- Anti-seize bases
- Copper-graphite, nickel-graphite, metal-free (graphite, ceramic), moly (MoS2), zinc, PTFE/food grade
- Typical upper temperature
- About 450 °C for moly up to about 1,315 °C for nickel grades (maker data)
- Nut factor K
- About 0.10 to 0.17 lubricated against about 0.20 dry (typical, varies by product)
- High-purity grades
- Nuclear grade nickel or metal-free with low chloride, fluorine and sulfur
- Thread sealants
- Anaerobic pipe sealants, threadlockers (low, medium, high strength), pipe dope
- PTFE tape
- 12, 19 and 25 mm widths; general, gas and oxygen-service grades
- Documents
- Safety data sheet, technical data sheet, batch test report where the grade has one

What we supply
- Anti-seize compounds
- Copper, nickel, metal-free and moly pastes in brush-top cans, tubes and aerosols
- High-purity grades
- Low halogen, low sulfur nickel or metal-free grades for stainless and nuclear-style specifications
- Anaerobic sealants
- Pipe thread sealants, threadlockers and primers for inactive metals
- PTFE thread seal tape
- General, gas and oxygen-service tape in common widths
- Pipe dope
- Thread sealing pastes for metal pipe threads
- With your bolting
- Packed with stud bolt kits for shutdowns, by joint or by unit
Anti-seize compound types compared
Choose the base for the metal, the temperature and the service. The figures below are typical values from maker data sheets and supplier guides; the product data sheet always governs.
| Type | Typical upper temperature | Typical nut factor K | Good for | Avoid or check |
|---|---|---|---|---|
| Copper-graphite | About 980 °C (1,800 °F) | 0.13 to 0.17 | Carbon and alloy steel studs, general plant work | Ammonia, acetylene and vinyl monomer service; aluminum; stainless where galvanic attack is a concern |
| Nickel-graphite | About 1,315 °C (2,400 °F); some grades higher | 0.12 to 0.16 | Stainless and nickel alloy bolting, high temperature, chloride environments | Food contact; projects that exclude nickel |
| Metal-free (graphite or ceramic) | Varies widely by maker; check the data sheet | About 0.16 to 0.18 (one maker) | Stainless steel, high-purity and nuclear-style specifications | Graphite in wet chloride service on carbon steel |
| Moly (MoS2) | About 450 °C (842 °F) in air | 0.10 to 0.13 | High-load threads where the lowest friction is wanted | Hot oxidizing conditions; using a dry torque value |
| Graphite | About 540 °C (1,000 °F) | 0.13 to 0.16 | Steam fittings, joints where metal particles are not wanted | Wet or marine conditions on carbon steel and aluminum |
| Zinc | About 400 °C (752 °F) | 0.14 to 0.17 | General low-temperature work | High temperature |
| PTFE or food grade | About 260 °C for PTFE pastes; food grades vary from about 200 to 400 °C | 0.12 to 0.14 (PTFE pastes) | Food, pharmaceutical and clean service | High-temperature bolting |
Temperatures and K values are typical figures from published maker data and supplier guides. They vary by product and by test method. Use the K value from the data sheet of the exact product you will apply. Confirm suitability for oxygen, chlorine or strong oxidizers with the maker.
How lubricant changes bolt torque: worked example
The short-form torque equation is T = K x D x F. For the same bolt load F, torque falls in direct proportion to the nut factor K. The rows below hold the bolt load constant and change only the lubricant.
| Thread condition | Nut factor K (typical) | 3/4-10 UNC stud, 16,700 lbf load | M20 stud, 49 kN load |
|---|---|---|---|
| Dry, as received | 0.20 | 209 ft-lbf (283 N·m) | 196 N·m |
| Copper anti-seize | 0.17 | 177 ft-lbf (241 N·m) | 167 N·m |
| Nickel anti-seize | 0.15 | 157 ft-lbf (212 N·m) | 147 N·m |
| Moly (MoS2) paste | 0.11 | 115 ft-lbf (156 N·m) | 108 N·m |
Illustrative only. 16,700 lbf is 50 ksi on the 0.334 sq in. stress area of a 3/4-10 UNC thread; 49 kN is 200 MPa on the 245 mm2 stress area of M20. Your joint procedure sets the target bolt load, and the lubricant maker’s data sheet gives K.
Anti-seize and sealants in Saudi plants
Heat, sand, coastal humidity and site rules shape how these products are bought and stored. This applies in Jubail Industrial City, Ras Al Khair and across the Eastern Province. We could not verify a Saudi Aramco or SABIC document that sets anti-seize selection, so check your project specification.
| Requirement | What it means |
|---|---|
| SASO and SABER | Importers register products in SABER, and every consignment needs a shipment certificate of conformity. Regulated products also need a product certificate. |
| Project specification | Your bolting procedure or line class may name the lubricant type, a K value, or a no-copper rule. That document governs. |
| Heat in storage | Maker data sheets set storage ceilings near 28 to 30 °C. Summer temperatures in Jubail run far above that, so store indoors and out of sun. |
| Sand and dust | Grit in an open tin turns anti-seize into a lapping paste. Keep lids shut and wipe threads before applying. |
| Coastal chlorides | Salt-laden air and humidity favor nickel or metal-free grades on stainless studs near the sea. |
| Hot units | Furnace, heater and steam flanges need a grade rated above the operating temperature, such as nickel-graphite. |
| Site HSE | Check whether your site needs the safety data sheet before the product goes on site, and keep it with the work pack. |
We do not cite a Saudi Aramco or SABIC document here because we could not verify one that covers anti-seize or thread sealant selection. Confirm requirements against your project specification and the current revision of any referenced standard.
Where anti-seize and thread sealants are used
The same plant uses several products, each for a different joint.
Flange stud bolts
Anti-seize on threads and nut faces gives a repeatable nut factor and easier break-out at the next shutdown.
Stainless and alloy bolting
Nickel or metal-free grades reduce galling on B8 and B8M studs and nickel alloy fasteners.
Hot joints
Heater, furnace, turbine and steam flanges where bolts must come apart after long heat exposure.
Pipe threads
Anaerobic sealant, PTFE tape or pipe dope on NPT and ISO 7 tapered threads for utilities and instruments.
Threadlocking
Anaerobic threadlockers stop vibration loosening on pump, motor and machinery fasteners.
Shutdown kits
Lubricant packed with stud bolt kits so every joint gets the product the torque table assumes.
Packed with your bolting
Lubricant is part of the joint. We can supply it with the studs, nuts and washers so the crew has the product the torque values were calculated for.
- Studs cut and threaded in our factory in Al-Jubail
- Lubricant type named per kit
- Brush-top cans for site use
- Matched to your torque table
Documents you can ask for
Chemical products ship with the maker’s documents. Bolting in the same order carries its own certificates.
- Safety data sheet (SDS)
- Technical data sheet
- Batch test report for high-purity grades
- EN 10204 3.1 for studs and nuts
- Third-party inspection on request
What an anti-seize compound does
An anti-seize compound separates mating threads with fine solid particles held in a grease or oil carrier. The solids carry the load where the grease would squeeze out. They keep the metal surfaces apart during tightening and after years in service.
Galling is the main reason to use it. Galling happens when tightening pressure breaks the oxide film on the threads and bare metal welds to bare metal. Austenitic stainless steel and nickel alloys are the most prone, especially stainless studs with stainless nuts.
The second reason is break-out. A flange opened after a run at high temperature, or after years in humid coastal air, often has corroded or fused threads. A good anti-seize leaves a film that lets the nut turn off without stripping the stud.
The third reason is control. Anti-seize gives a more consistent friction value than dry or rusty threads. A consistent nut factor means torque turns into bolt load more predictably, which is the point of a torque procedure.
What anti-seize is not
Anti-seize is not a thread sealant, a threadlocker or a gasket compound. It does not cure and it does not lock the nut. Do not put it on threads that are meant to be locked with an anaerobic threadlocker, because the two products cancel each other.
How to choose an anti-seize compound
Choose an anti-seize compound by the bolt material, the maximum service temperature, the process fluid and any purity limits in your specification. Then use the K value of that exact product in the torque calculation.
Copper-graphite is the usual general-purpose grade for carbon and alloy steel studs such as ASTM A193 B7. Typical data sheets rate it to about 980 °C (1,800 °F).
By bolt material
Most guides recommend nickel or metal-free grades for stainless steel and nickel alloys. Copper grades are aimed at carbon and alloy steel.
- Carbon and alloy steel (B7, B16, L7): copper-graphite or moly for general service; nickel for very hot joints.
- Austenitic stainless (B8, B8M): nickel-graphite or a metal-free grade.
- Nickel alloys (Alloy 625, 825, C-276 type bolting): nickel or metal-free; follow the project’s purity limits.
- Aluminum parts: avoid copper grades. Aluminum is anodic to copper, so the aluminum part corrodes if moisture gets in.
By temperature
Rate the compound above the highest metal temperature the bolt will see, not the process design temperature on paper. Typical limits are about 450 °C in air for moly and 540 °C for graphite. Copper reaches about 980 °C and nickel about 1,315 °C.
By service
Some services rule out whole families of product. Check the process fluid against the data sheet before you choose on temperature alone.
- Ammonia, acetylene and vinyl monomers: copper-free grade.
- Oxygen-rich service and chlorine or strong oxidizers: many ordinary anti-seize data sheets exclude these; use only a product the maker states is suitable.
- Food and pharmaceutical: a food-grade compound; check its temperature rating, which is usually lower than copper or nickel grades.
- Nuclear-style or high-purity specifications: a grade with published chloride, fluorine and sulfur limits.
- Identify the stud and nut grades on the joint list.
- Find the maximum metal temperature at the bolt.
- Check the process fluid and any no-copper, no-nickel or purity rule.
- Pick the base: copper, nickel, metal-free, moly or food grade.
- Take K from that product’s data sheet and calculate torque.
- Write the product type and K on the joint record.
Copper, nickel or metal-free: service restrictions
Copper anti-seize is avoided on stainless steel in many plants, and in a few services it is excluded outright. The reasons are galvanic corrosion risk, chemical reactions with copper and purity limits.
Copper on stainless steel
Copper-based compounds can cause galvanic corrosion in some stainless and galvanized systems. One lubricant maker says this is rare and is mostly linked to low-quality compounds that dry out or wash out.
Even so, maker literature steers stainless bolting to nickel-bearing or metal-free grades. One maker’s catalogue describes its nickel grade as safe on stainless steel above 288 °C (550 °F). Many project specifications simply ban copper on stainless studs, which removes the argument.
Ammonia, acetylene and vinyl monomers
These chemicals are unstable in the presence of copper. Maker literature recommends copper-free nickel grades for them. Ammonia plants, acetylene lines and vinyl chloride units should therefore be treated as no-copper areas for anti-seize.
Oxygen and strong oxidizers
Petroleum-carried pastes are generally not for oxygen-rich systems. One stainless-steel anti-seize data sheet states it is not recommended for pure oxygen or oxygen-rich systems, nor for chlorine or other strong oxidizers. Use only lubricants the maker states are suitable for oxygen service.
Nuclear grade and high-purity anti-seize
Nuclear grade means a compound made with the lowest practical levels of halogens, sulfur and heavy metals, including copper. The aim is to avoid stress corrosion of stainless steel and alloy bolting in service.
One maker’s high-purity nickel grade publishes limits of 50 ppm chloride, 200 ppm fluorine and 100 ppm sulfur, rated to 1,315 °C. Its metal-free high-purity grade lists the same limits. These are typical published values, not a universal standard.
Ask for a batch test report when your specification sets numeric limits. Makers of these grades typically test each batch against their own material specification.
Nut factor K: why lubricant changes bolt torque
The lubricant on the threads and under the nut sets how much of the applied torque becomes bolt load. Change the lubricant and the same torque gives a different bolt load.
The short-form equation is T = K x D x F. T is torque, D is nominal bolt diameter, F is the bolt load you want and K is the nut factor. K is measured, not calculated, and it bundles thread friction, nut-face friction and geometry into one number.
A NASA technical memorandum on lubricated bolts gives 0.2 as a recommended K for dry fasteners and 0.1 for lubricated ones. Maker data sits between: one maker’s nickel paste measured 0.15 on steel and 0.16 on 304 stainless, and its copper paste 0.17. The same maker measured 0.27 on solvent-cleaned, unlubricated steel, so dry is not a fixed value either.
Worked example: 3/4 in. B7 stud
Take a 3/4-10 UNC stud with a tensile stress area of 0.334 sq in. Suppose the procedure asks for 50 ksi bolt stress. The target bolt load is 50,000 x 0.334 = 16,700 lbf.
Dry, with K = 0.20: T = 0.20 x 0.75 x 16,700 = 2,505 lbf-in, or 209 ft-lbf. With nickel anti-seize at K = 0.15 the torque falls to 157 ft-lbf. With moly paste at K = 0.11 it falls to 115 ft-lbf.
Now the mistake. Suppose the crew applies the dry value of 209 ft-lbf to studs coated in moly paste. The load becomes 2,505 / (0.11 x 0.75) = 30,400 lbf. That is about 91 ksi, or roughly 87% of the 105 ksi minimum yield of B7. The gasket may be crushed and the stud is close to yield.
Rules that follow from the example
- Calculate torque with the K of the product actually used, not a generic table.
- Lubricate the nut bearing face as well as the threads, because nut-face friction is part of K.
- Never mix anti-seize types on the same joint.
- Record the lubricant and K on the joint record so the next crew repeats it.
- ASME PCC-1 includes an appendix on nut factor calculation of target torque; use it with your own procedure.
Applying anti-seize to flange stud bolts
Apply anti-seize to clean threads, along the full engaged length, and to the nut face that turns against the flange or washer. A thin, even film works better than a thick layer.
Coated studs need a check first. One bolting guide lists fluoropolymer-coated studs among the cases where anti-seize is not added, because the coating already sets the friction. Follow the coating maker’s data and your procedure rather than adding paste by habit.
Common mistakes
- Using a dry torque table with lubricated studs.
- Lubricating threads only and leaving the nut face dry.
- Mixing a copper paste on one side of a joint and nickel on the other.
- Letting compound reach the gasket, where it can affect sealing.
- Using copper paste on stainless studs where the specification forbids it.
- Leaving tins open in dusty areas, so grit gets into the paste.
- Putting anti-seize on threads that need a threadlocker.
- Clean the stud threads, nuts and flange spot faces of old compound, sand and rust.
- Check that each nut runs freely by hand along the stud.
- Stir the compound if it has settled, and use a clean brush.
- Coat the threads over the length the nuts will engage, on both ends of the stud.
- Coat the nut face that will turn against the flange or the washer.
- Keep compound off the gasket and the flange sealing faces.
- Run the nuts on, then tighten in the pattern and passes your procedure sets.
- Close the tin straight away and record the product used.
Anaerobic thread sealants and threadlockers
Anaerobic products are liquid resins that stay fluid in air and cure to a hard plastic when confined between metal threads. They need two things to cure: no air and metal ions from the part surface.
Thread sealants fill the spiral leak path of tapered pipe threads. Threadlockers fill the clearance of bolt and screw threads so vibration cannot turn the nut. The chemistry is similar, but the products are formulated differently, so use each for its own job.
Cure, primers and temperature
On active metals such as carbon steel, brass and copper, handling strength typically comes in 10 to 20 minutes. Full cure takes about 24 hours. Pressurize only after the cure time on the data sheet.
Inactive surfaces cure slowly or not at all. These include stainless steel, zinc and galvanized coatings, anodized aluminum and passivated parts. A primer or activator brushed on first speeds the cure.
Cure slows below about 15 °C and speeds up above 25 °C. In Saudi summer heat, work quickly once the product is on the threads.
One engineering guide gives anaerobic pipe sealants a typical limit of about 150 °C (300 °F) and pressures up to 10,000 psi. Check the exact product; some grades go higher.
Threadlocker strengths
Threadlockers come in low, medium and high strength, plus a thin wicking grade. Purple, blue, red and green are a common color code, but not every maker follows it. Order by strength and data sheet, not by color.
- Low strength: small screws and adjusters; removes easily with hand tools.
- Medium strength: general bolts and studs that must come apart for maintenance with hand tools.
- High strength: permanent assemblies; removal typically needs local heat of about 250 °C.
- Wicking grade: low-viscosity liquid applied to parts that are already assembled.
Where not to use anaerobics
- On plastic threads, unless the data sheet says the product is compatible; some anaerobics attack thermoplastics.
- In oxygen service, unless the maker states the product is suitable.
- On flange studs that must be torqued to a set bolt load; use anti-seize there.
PTFE thread seal tape
PTFE thread seal tape is unsintered PTFE film wrapped on male tapered pipe threads. It fills the thread gaps and lubricates assembly so the threads can be drawn tighter.
Use it only on tapered threads that seal on the threads: NPT to ASME B1.20.1 and ISO 7-1 R, Rc and Rp threads. ISO 228-1 G parallel threads do not seal on the thread and need a gasket or other external seal.
Do not use tape on flared, coned or tube fitting ends. A 37° flare fitting seals on its flare seat, and a compression fitting seals on its ferrules. Tape on those threads seals nothing and can shed fragments into the line.
Density, thickness and width
Tape density varies by grade. One maker’s general-purpose tape lists 0.5 to 0.95 g/cm3 at 0.075 mm thick. High-density oxygen tapes are sold at up to about 1.5 g/cm3 and about 0.1 mm thick. Denser tape needs fewer wraps.
Common widths are 12, 19 and 25 mm. One fitting maker recommends 1/4 in. tape for 1/8 to 3/8 in. pipe threads and 1/2 in. tape for 1/2 in. and larger.
Standards and color codes
EN 751-3 covers unsintered PTFE tapes and strings for metallic threaded joints in gas and hot water service. It has classes for fine and coarse threads, and its scope runs from -20 °C to 125 °C.
A-A-58092, a US Commercial Item Description, covers PTFE tape for liquid and gaseous oxygen systems. Some fitting makers supply tape conforming to it.
Color codes are regional conventions. Yellow is used for gas tape in some countries, and green is common for oxygen tape in the US. White tape is general purpose. Always confirm the grade on the reel, not the color.
Oxygen-service tape
Oxygen-service tape is pure PTFE made without lubricant residue that could react with oxygen. One maker’s tape is rated suitable for oxygen with residual lubricant below 0.1% by mass. Some oxygen tapes carry BAM test approval. Keep oxygen tape sealed and clean until use.
- Clean male and female threads and remove old tape or compound.
- Start at the first thread, keeping the tape edge back so nothing overhangs the pipe end.
- Wrap in the direction of the thread spiral, so tightening does not unwind the tape.
- Apply two to three turns of standard tape, pulled snug so it takes the thread form.
- Press down loose edges, assemble, and do not back off to align; re-make the joint instead.
| Grade | Typical density | Typical thickness | Use | Notes |
|---|---|---|---|---|
| General purpose (white) | About 0.5 to 0.95 g/cm3 | About 0.075 mm | Water, air, general utilities | Not for gas lines where gas tape is required |
| Gas grade (often yellow) | Varies by maker | About 0.1 mm | Fuel gas and LPG threads | Approved to the national gas standard where required |
| Oxygen service (often green) | Up to about 1.5 g/cm3 | About 0.09 to 0.1 mm | Oxygen and oxygen-enriched lines | Lubricant-free; check oxygen approval on the reel |
Values are typical published maker figures. Tape service temperature is commonly quoted up to 232 to 260 °C by makers; EN 751-3 tests cover -20 to 125 °C for gas and hot water. Never use tape on hydraulic fittings that seal on a seat or face.
Pipe dope and choosing a pipe thread sealant
Pipe dope is a thread sealing paste brushed onto male pipe threads. Some are solvent-based and harden as the solvent evaporates. Others contain PTFE or cure anaerobically, so read the data sheet to see which kind you have.
Solvent-based dope is cheap and works on most pipe materials, but it shrinks as it dries. Shrinkage, heat aging and vibration can open leak paths, so it suits low-pressure, low-temperature utility work.
For process and instrument lines the choice is usually between PTFE tape and an anaerobic sealant. Tape is clean and quick. Anaerobic sealant fills the whole thread, resists vibration and cannot shed strands into the line.
Tape or paste on instrument fittings
Instrument technicians usually wrap two or three turns of tape on NPT male threads. Excess tape or paste is a real risk here, because fragments can block needle valve ports and gauge accessories downstream.
| Factor | PTFE tape | Solvent pipe dope | Anaerobic sealant |
|---|---|---|---|
| How it seals | Fills thread gaps, lubricates assembly | Paste hardens as solvent evaporates | Liquid cures to plastic in the threads |
| Vibration | Low resistance | Low resistance | Good resistance |
| Shrinkage | None | Shrinks as it dries | None (no solvent) |
| Adjust after assembly | Do not back off | Only for a few minutes | Allowed until it cures |
| Contamination risk | Strands can shed into the line | Excess paste can enter the line | Excess paste can enter the line |
| Time to pressure | Immediate | Short | Up to about 24 hours for full cure |
| Typical use | Utilities, instrument threads, oxygen with the right tape | Low-pressure utilities | Process, hydraulic and vibrating pipework |
Summarized from engineering guides on pipe thread sealant selection. Product data sheets give the actual temperature and pressure limits.
Storage, shelf life and reading the safety data sheet
Store anti-seize and sealants indoors, sealed, in a cool and dry place. Anti-seize data sheets give optimal storage of about 8 to 21 °C or 10 to 25 °C. They warn that storage above 28 to 30 °C can affect the product.
Anaerobic bottles are never full, because the air space stops the liquid curing in the bottle. Do not pour used product back into the container. PTFE tape has a very long shelf life but should stay in its sleeve, clean and dry.
The 16 sections of an SDS
A GHS-format safety data sheet has 16 sections in a fixed order. You do not need to read all of them every time. For thread compounds, these are the ones that matter on site.
- Section 1, Identification: product name and maker, so you know the SDS matches the tin.
- Section 2, Hazard identification: signal word, pictograms and hazard statements.
- Section 3, Composition: metals, solvents or resins present, such as nickel or copper powder.
- Section 7, Handling and storage: storage temperature and incompatible materials.
- Section 8, Exposure controls: gloves, eye protection and ventilation.
- Section 9, Physical and chemical properties: flash point for aerosols and solvent products.
- Section 10, Stability and reactivity: what the product must not contact, such as oxidizers.
- Section 13, Disposal: how to dispose of rags, brushes and part-used tins.
- Section 14, Transport: needed for aerosols and some solvent sealants.
SDS and TDS are different
The safety data sheet covers hazards and handling. The technical data sheet covers performance: temperature range, K value, cure times and approvals. You need both to choose and use a product correctly.
RFQ checklist and checks on receipt
A clear request gets the right product on the first quote. Give the joint and service details, not only a product name, and we will match a suitable grade from established manufacturers.
We do not quote brands as stocked. If your specification names a product, send the specification clause and we will offer that product or a documented equivalent for your approval.
What to include in your RFQ
- Product family: anti-seize, anaerobic pipe sealant, threadlocker, PTFE tape or pipe dope.
- For anti-seize: base (copper, nickel, metal-free, moly) and any no-copper or high-purity rule.
- Bolt and nut grades, for example B7/2H or B8M/8M.
- Maximum metal temperature at the joint and the process fluid.
- Purity limits with numbers, for example chloride, fluorine and sulfur in ppm, and whether a batch test report is needed.
- For PTFE tape: width, grade (general, gas, oxygen) and thread type (NPT or ISO 7).
- For anaerobics: strength, thread size range and whether a primer is needed for stainless or plated parts.
- Pack size (brush-top can, tube, aerosol, bulk) and quantity.
- Documents: SDS, TDS, batch test report, and any third-party inspection.
Checks on receipt
- Label matches the order: product type, grade and pack size.
- Batch number and manufacture or expiry date are legible and within shelf life.
- SDS and TDS received and match the product.
- Containers sealed, undamaged and not stored in sun on arrival.
- Batch test report received where purity limits apply.
Anti-seize and thread sealant questions
What is anti-seize compound used for?
Anti-seize compound is a paste of metal, graphite or ceramic solids in a grease carrier. It is brushed on bolt threads and nut faces to prevent galling during tightening and seizing in service. It also gives a more consistent nut factor, so torque turns into bolt load more predictably. It is widely used on flange studs, stainless fasteners and hot joints that must be opened at the next shutdown.
Copper or nickel anti-seize: which should I use?
Use copper-graphite on carbon and alloy steel studs such as B7 for general service. Use nickel-graphite or a metal-free grade on stainless steel and nickel alloys, at very high temperature, and in ammonia, acetylene or vinyl monomer service. Copper is typically rated to about 980 °C and nickel to about 1,315 °C. Always follow any no-copper rule in your project specification.
Why is copper anti-seize avoided on stainless steel?
Copper-based compounds can cause galvanic corrosion in some stainless and galvanized systems, especially if the compound dries out or washes away. Maker literature therefore points stainless bolting to nickel or metal-free grades, and many specifications ban copper on stainless studs. Copper is also excluded where ammonia, acetylene or vinyl monomers are present, because these are unstable in contact with copper.
What is nuclear grade anti-seize?
Nuclear grade anti-seize is a high-purity compound made with the lowest practical levels of halogens, sulfur and heavy metals, including copper. It is used on stainless steel and alloy bolting to avoid stress corrosion. One maker publishes limits of 50 ppm chloride, 200 ppm fluorine and 100 ppm sulfur. Ask for a batch test report when your specification sets numeric limits.
How much should I reduce torque when using anti-seize?
Do not use a fixed percentage. Calculate torque from T = K x D x F using the K value on the data sheet of the product you apply. Typical K is about 0.20 dry and about 0.11 to 0.17 with anti-seize. Torque for the same bolt load can therefore fall by roughly 15 to 45 percent. Our bolt torque calculator lets you enter your own K.
What is the nut factor K?
The nut factor K is an experimentally measured constant in the torque equation T = K x D x F. It combines thread friction, nut-face friction and thread geometry. K depends on the lubricant, the coating, the surface finish and the bolt material. One maker measured 0.15 for a nickel paste on steel and 0.27 for clean dry steel. K must match the actual condition.
What happens if I use dry torque values on lubricated studs?
The bolts are over-loaded. Take our 3/4 in. B7 example. A dry torque of 209 ft-lbf applied over moly paste gives about 91 ksi instead of 50 ksi. That is roughly 87 percent of B7 minimum yield. That can crush the gasket, damage the flange or yield the stud. Always match the torque table to the lubricant.
Can I use anti-seize on PTFE-coated stud bolts?
Check first. Fluoropolymer coatings already lower friction, and one bolting guide lists coated studs among the cases where anti-seize is not added. Adding paste would change K again. Follow the coating maker’s data and your bolting procedure, and record the condition used. If the procedure does call for a lubricant on coated studs, use the K for that combination.
What is the difference between a thread sealant and a threadlocker?
Both are usually anaerobic resins that cure between metal threads without air. A thread sealant fills the leak path of tapered pipe threads so fluid cannot escape. A threadlocker fills the clearance of bolt and screw threads so vibration cannot loosen the nut. They are formulated for different jobs, so use the product made for the joint you are assembling.
Do anaerobic sealants work on stainless steel?
Yes, but slowly without help. Stainless steel, zinc and galvanized coatings, anodized aluminum and passivated parts are inactive surfaces with few free metal ions. Cure is slow or incomplete. Brush on the primer or activator the maker recommends, let it dry, then apply the sealant. Allow the full cure time before pressurizing, typically about 24 hours.
How many wraps of PTFE tape should I use on pipe threads?
Two to three turns of standard tape is the usual practice, wrapped in the direction of the thread spiral and pulled snug. Start at the first thread without letting tape overhang the pipe end. Denser tapes need fewer turns. Too much tape stops the threads engaging fully and can shed strands into the line.
Can PTFE tape be used on compression or flare fittings?
No. Fitting makers say tape should be used only on male tapered pipe threads, not on flared, coned or tube fitting ends. A 37° flare seals on its seat and a compression fitting seals on its ferrules, not on the threads. Tape there does nothing useful and fragments can enter the system.
Which PTFE tape is used for oxygen service?
Use tape made and packed for oxygen service: pure PTFE without lubricant residue, often colored green in US practice and sometimes BAM tested. A-A-58092 is a US Commercial Item Description for PTFE tape in liquid and gaseous oxygen systems. Keep the tape sealed until use and check the oxygen approval on the reel, not just the color.
How should anti-seize be stored in Saudi heat?
Store it indoors in a closed, air-conditioned store if possible, out of direct sun. Maker data sheets give optimal storage around 8 to 25 °C and warn against storage above 28 to 30 °C. Keep lids shut against sand and dust, stir settled paste before use, and never return used material to the original container.
Updated
Related
B8 and B8M stud bolts
Stainless studs that need anti-seize against galling.
PTFE coated stud bolts
Fluoropolymer coated studs with low, stable friction.
Torque wrenches and tensioners
Tools to apply the torque your nut factor sets.
Send your lubricant and sealant list
Tell us the bolt grades, temperature and service, or send the specification clause. We quote suitable anti-seize, sealants and tape with SDS and data sheets, alone or packed with your bolting.